Treatment Agent For Copper And Copper Alloy

Treatment procedure
���

Degreasing powder

CF NO.
Using method
Characteristic
 
Concentration(%)
Temperature(°C)
Time(min)
 
103
3~5

Normal temperature~50

5~10

It has a strong power of degreasing, and it will not corrode its surface by using immersion.

155
3~5

Normal temperature~50

5~10

It has a strong power of degreasing, and it will not corrode its surface by using immersion.

Eliminate rust and chemical grinding agent

CF NO.
Using method
Characteristic
 
Concentration(%)
Temperature(°C)
Time(min)
 
820
5

Normal temperature

1~4

It is an eliminating rust of copper and copper alloy by using immersion.

832
5

45~50

5~10

It is an eliminating rust of copper and copper alloy by using immersion.

850
50

Normal temperature

1~3

It is a chemical grinding of copper and copper alloy by using immersion.

Protected filming agent

CF NO.
Using method
Characteristic
 
Concentration(%)
Temperature(°C)
Time(min)
 
800
5

Normal temperature

5’~30′

It can protect the surface of copper and copper alloy to avoid erosion.